| Nickel Alloys |
| Nickel 200 |
Commercially pure nickel most widely used grade used in corrosive environments at both high and low generally specified for transistor caps, electronic tubes, leads of electronic components / lead-in-wires for lamps and for wire-mesh |
- Food processing equipment
- Shipping drums for chemicals
- Caustic handling equipment
- Aerospace and missile components
- Electronic parts
|
| Nickel 201 |
Increased ductility preferred for applications involving exposure to high temperatures |
- Caustic evaporators
- Plater bars
- Combustion boats
|
| Hastelloy Nickel-Molybdenum Alloy |
| Inconel 600 Inconel 601 |
Used in severely corrosive environs at elevated temperatures Resistant to oxidation to 2150f Excellent mechanical properties |
- Chemical & food processing equipment
- Heat exchanger tubing
- Furnace parts
- Bellows
- Electronic components,
- Aircraft parts
- Springs
|
| Inconel 617 |
Optimum high-temperature mechanical stability Oxidation and corrosion resistance. excellent cyclic oxidation and carburization resistance at 2000f Good stress rupture properties above 1800f |
- Aerospace and engine components
- After-burners
- Flame holders
- Spray bars
- Combustion liners
- Turbine seals
- Heat-treating equipment
- Nitric acid catalyst supports
|
| Inconel 625 |
Outstanding resistance to corrosion and oxidation Exceptional fatigue strength |
- Aerospace ducting systems
- Combustion systems
- Thrust reverser assemblies
- After-burners
- Fuel nozzles
- Hot brine handling equipment
- Chemical equipment
- Spray bars
|
| Inconel 718 Inconel 722 |
Excellent oxidation resistance to 1800f Excellent strength from - 425f to +1200f Age hardenable and weldable in fully aged condition |
- Jet engines,
- Pump bodies and parts
- Rocket motors and trust reversers
- Hot extrusion tooling
|
| Inconel X750 |
Age hardenable alloy with good corrosion & oxidation resistance also good relaxation resistance |
- Gas turbine parts
- Steam service and nuclear reactor springs & bolts
- Vacuum envelopes
- Extrusion dies
- Bellows
- Forming tools
|
| Monel Nickel-Copper Alloy |
| Monel 400 Monel 405 Monel K500 |
High strength Excellent corrosion resistance and toughness over a wide temperature range Highly resistant to corrosion by chlorinated solvents, glass-etching agents, sulfuric acid and most alkalies |
- Valves
- Pumps
- Pump and propeller shafts
- Marine fixtures
- Electrical and electronic components
- Process equipment
- Petroleum refining and production equipment
- Heat exchangers
- Screw machine products
- Water meter parts
|
| Incoloy Nickel-Iron-Chromium-Iron |
| Incoloy 800 Incoloy 825 |
Resistant to oxidation and carburization at elevated temperatures Resists stress-corrosion cracking, sulfur attack, internal oxidation and scaling in a wide range of industrial atmospheres |
- Heat exchanger tubing
- Petrochemical flares and process piping
- Furnace brackets, baskets & trays
- Chemical and power plant
- Superheater and reheater tubing
|
| Waspaloy |
|
|